CuSn10-C (CC480K)
Grade : | CuSn10-C |
Number: | CC480K |
Classification: | Copper-tin alloy |
Chemical composition % of grade CuSn10-C ( CC480K )
Fe | Si | Mn | Ni | P | S | Al | Cu | Pb | Zn | Sb | Sn | - |
max 0.2 | max 0.02 | max 0.1 | max 2 | max 0.2 | max 0.05 | max 0.01 | 88 - 90 | max 1 | max 0.5 | max 0.2 | 9 - 11 | Cu including Ni |
Mechanical properties of grade CuSn10-C ( CC480K )
Rm - Tensile strength (MPa) (GS) | 250 |
Rm - Tensile strength (MPa) (GM) | 270 |
Rm - Tensile strength (MPa) (GC) | 280 |
Rm - Tensile strength (MPa) (GZ) | 280 |
Rp0.2 0.2% proof strength (MPa) (GS) | 130 |
Rp0.2 0.2% proof strength (MPa) (GM) | 160 |
Rp0.2 0.2% proof strength (MPa) (GC) | 170 |
Rp0.2 0.2% proof strength (MPa) (GZ) | 160 |
A - Min. elongation at fracture (%) (GS) | 18 |
A - Min. elongation at fracture (%) (GM) or (GC) or (GZ) | 10 |
Brinell hardness (HBW): (GS) | 70 |
Brinell hardness (HBW): (GM) or (GC) or (GZ) | 80 |