Send Message In Whatsapp
CuSn10Pb10-C (CC495K)
Grade : | CuSn10Pb10-C |
Number: | CC495K |
Classification: | Copper-tin-lead alloy |
Chemical composition % of grade CuSn10Pb10-C ( CC495K )
Fe | Si | Mn | Ni | P | S | Al | Cu | Pb | Zn | Sb | Sn | - |
max 0.25 | max 0.01 | max 0.2 | max 2 | max 0.1 | max 0.1 | max 0.01 | 78 - 82 | 8 - 11 | max 2 | max 0.5 | 9 - 11 | Cu including Ni |
Mechanical properties of grade CuSn10Pb10-C ( CC495K )
Rm - Tensile strength (MPa) (GS) | 180 |
Rm - Tensile strength (MPa) (GM) or (GZ) or (GC) | 220 |
Rp0.2 0.2% proof strength (MPa) (GS) | 80 |
Rp0.2 0.2% proof strength (MPa) (GM) or (GZ) or (GC) | 110 |
A - Min. elongation at fracture (%) (GS) or (GC) | 8 |
A - Min. elongation at fracture (%) (GM) | 3 |
A - Min. elongation at fracture (%) (GZ) | 6 |
Brinell hardness (HBW): (GS) | 60 |
Brinell hardness (HBW): (GM) | 65 |
Brinell hardness (HBW): (GZ) or (GC) | 70 |