CuSn7Zn4Pb7-C (CC493K)
Grade : | CuSn7Zn4Pb7-C |
Number: | CC493K |
Classification: | Copper-tin-lead alloy |
Chemical composition % of grade CuSn7Zn4Pb7-C ( CC493K )
Fe | Si | Ni | P | S | Al | Cu | Pb | Zn | Sb | Sn | - |
max 0.2 | max 0.01 | max 2 | max 0.1 | max 0.1 | max 0.01 | 81 - 85 | 5 - 8 | 2 - 5 | max 0.3 | 6 - 8 | Cu including Ni |
Mechanical properties of grade CuSn7Zn4Pb7-C ( CC493K )
Rm - Tensile strength (MPa) (GS) or (GM) | 230 |
Rm - Tensile strength (MPa) (GZ) or (GC) | 260 |
Rp0.2 0.2% proof strength (MPa) (GS) or (GM) | 120 |
Rp0.2 0.2% proof strength (MPa) (GZ) or (GC) | 120 |
A - Min. elongation at fracture (%) (GS) | 15 |
A - Min. elongation at fracture (%) (GM) or (GZ) or (GC) | 12 |
Brinell hardness (HBW): (GS) or (GM) | 60 |
Brinell hardness (HBW): (GZ) or (GC) | 70 |