Send Message In Whatsapp
CuZn35Ni3Mn2AlPb (CW710R)
Grade : | CuZn35Ni3Mn2AlPb |
Number: | CW710R |
Classification: | Complex copper-zinc alloy |
Chemical composition % of grade CuZn35Ni3Mn2AlPb ( CW710R )
Fe | Si | Mn | Ni | Al | Cu | Pb | Sn | Others | - |
max 0.5 | max 0.1 | 1.5 - 2.5 | 2 - 3 | 0.3 - 1.3 | 58 - 60 | 0.2 - 0.8 | max 0.5 | total 0.3 | Zn - remainder |
Mechanical properties of grade CuZn35Ni3Mn2AlPb ( CW710R )
Rm - Tensile strength (MPa) (R490) | 490 |
Rm - Tensile strength (MPa) (R550) | 550 |
Rp0.2 0.2% proof strength (MPa) (R490) | 300 |
Rp0.2 0.2% proof strength (MPa) (R550) | 400 |
A - Min. elongation at fracture (%) (R490) | 20 |
A - Min. elongation at fracture (%) (R550) | 10 |
Brinell hardness (HB): (H120)(R490) | 120 - 150 |
Brinell hardness (HB): (H150)(R550) | 150 |